Specific Process Knowledge/Characterization/XRD/XRD SmartLab: Difference between revisions
| Line 20: | Line 20: | ||
The measurement settings and results of the pre-acceptance test are described in this document, also found on the Cleanroom drive: | The measurement settings and results of the pre-acceptance test are described in this document, also found on the Cleanroom drive: | ||
[https://labmanager.dtu.dk/view_binary.php?fileId=5413|(FAT) Factory Acceptance Test] - requires login | *[https://labmanager.dtu.dk/view_binary.php?fileId=5413|(FAT) Factory Acceptance Test] - requires login | ||
The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here: [[:File:Inspection certificate.pdf]] | The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here: [[:File:Inspection certificate.pdf]] | ||
Revision as of 21:17, 1 February 2023
Feedback to this page: click here
XRD SmartLab
The Rigaku SmartLab is an advanced XRD for measuring on thin films. All thin films can be measured without fixating the sample, as the system has a so called In-Plane arm.

The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:
XRD SmartLab in LabManager - requires login
Various measurement types including X-Ray reflectivity, Rocking curve, Theta-2theta, and Pole figures are described here:
The measurement settings and results of the pre-acceptance test are described in this document, also found on the Cleanroom drive:
- Factory Acceptance Test - requires login
The same measurement were completed as part of the acceptance, but no report was generated. In addition the inspection certificate is available here: File:Inspection certificate.pdf
Software for analysis
Please see the Data Analysis section at the main XRD page.
Characterization of thin films using X-ray reflectivity (XRR)
Implementing the XRR method the user can calculate thickness, density, and roughness of the deposited material. The XRR is also widely employed for multilayer stack analysis.
Here are some results available:
- Characterization of e-beam deposited Al thin films.
- Characterization of DC sputtered Al thin films.
- Characterization of ALD deposited Al2O3 and TiO2 ultrathin layers.
- Characterization of Sputtered deposited CrSi bilayer.
- Characterization of Sputtered deposited MgO thin films.
| Equipment | XRD SmartLab | |
|---|---|---|
| Purpose | Crystal structure analysis and thin film thickness measurement |
|
| X-ray generator |
Maximum rated output |
3 kW |
|
Rated tube voltage |
20 to 45 kV | |
|
Rated tube current |
2 to 60 mA | |
|
Type |
Sealed tube | |
|
Target |
Cu | |
|
Focus size |
0.4 mm x 8 mm (Line/Point) | |
| Goniometer |
Scanning mode |
incident / receiver coupled or independent |
|
Goniomenter radius |
300 mm | |
|
Minimum step size |
0.0001° (0.36") | |
|
Sample stage |
| |
|
Sample size |
Diameter: 150 mm Thickness: 0~21 mm | |
| Optics | Incident side |
|
| Receiver side |
| |
| Substrates | Substrate size |
up to 150 mm wafers |
| Allowed materials |
All materials | |