Jump to content

Specific Process Knowledge/Characterization/XRD/XRD Powder/XRD Powder software: Difference between revisions

From LabAdviser
Reet (talk | contribs)
new software page for XRD powder
 
Reet (talk | contribs)
Line 8: Line 8:


====For data analysis====
====For data analysis====
We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument, which can be accessed remotely.  
We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument, which can be accessed remotely. For more info about this software including how to access it remotely
[[Specific Process Knowledge/Characterization/XRD/HighScore analysis|click here.]]


====Additional software for measurements in a heated atmosphere====
====Additional software for measurements in a heated atmosphere====
If you are going to make measurements in a heated N<sub><sub>2</sub></sub> atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.
If you are going to make measurements in a heated N<sub><sub>2</sub></sub> atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.

Revision as of 13:09, 8 July 2022

Feedback to this page: click here

Software for the XRD Powder

For data export

On the Cleanroom drive you can find the DataViewer software, which is a very basic program that allows you to view your measurement results and export to other formats, e.g., csv or txt. To install DataViewer, go to the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\XRDMP and click "setup" (XRDMP stands for XRD Measurement Program). This will open a menu that allows you to install both DataViewer and XRDMP Creator. Just choose to install DataViewer. XRDMP Creater is only needed if you have made an agreement with the equipment responsible that you are allowed to create your own measurement routines.

For data analysis

We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument, which can be accessed remotely. For more info about this software including how to access it remotely click here.

Additional software for measurements in a heated atmosphere

If you are going to make measurements in a heated N2 atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.