Specific Process Knowledge/Thermal Process/C4 Aluminium Anneal furnace: Difference between revisions
Appearance
| Line 10: | Line 10: | ||
The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium or ALD oxides Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub>. | The Aluminium Anneal furnace (C4) is a Tempress horizontal furnace for annealing of silicon wafers with aluminium or ALD oxides Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub>. | ||
This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom B-1. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager before you use the furnace. | This furnace is the lowest of the furnace tubes in the furnace C-stack positioned in cleanroom B-1. In this furnace allowed to process wafers that contain aluminium. Please check the cross contamination information in LabManager, before you use the furnace. | ||
'''The user manual, technical information and contact information can be found in LabManager:''' | '''The user manual, technical information and contact information can be found in LabManager:''' | ||