| colspan="3"| C<sub>4</sub>F<sub>8</sub> (H2 currently fitted but closed) : 0 sccm | | colspan="3 "| C<sub>4</sub>F<sub>8</sub> (H2 currently fitted but closed) : 0 sccm | ||
|- | |- | ||
| SF6: 50 sccm | | SF6: 50 sccm |
Revision as of 09:59, 14 December 2020
Feedback to this page: click here
This system is a research tool and not available to the users
If you want to get access to the tool, then talk to professor Henry Jansen
Current setup and rules on Pegasus 2
Click here to access older configurations.
The current configuration is
Item | The currently applied modification | Comments |
---|---|---|
Available gasses and gas chemistry | { | OnlySF6 and O2 are used for Si, PR, and Cr etch. The rest is only make-up
{ |