====For data analysis====
====For data analysis====
We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument.
We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument, but will become available on a remote computer.


====Additional software for measurements in a heated atmosphere====
====Additional software for measurements in a heated atmosphere====