In 2010 DTU Nanolab acquired DRIE-Pegasus 1 (at the time called Danchip and DRIE-Pegasus, respectively). As a state-of-the-art etch tool with excellent performance and great flexibility, it grew immensely popular and by 2015 it was apparent that we needed yet another tool to cope with the demand. Therefore, in 2016 Pegasus 2 was acquired from a closed-down lab in Morocco and installed next to Pegasus 1. | In 2010 DTU Nanolab acquired DRIE-Pegasus 1 (at the time called Danchip and DRIE-Pegasus, respectively). As a state-of-the-art etch tool with excellent performance and great flexibility, it grew immensely popular and by 2015 it was apparent that we needed yet another tool to cope with the demand. Therefore, in 2016 Pegasus 2 was acquired from a closed-down lab in Morocco and installed next to Pegasus 1. | ||
Looking to expand our dry etching capabilities in 2017 we got an irresistible offer on a twin Pegasus system with cassette to cassette vacuum robot from a commerciel fab. The twin Pegasus system ( | Looking to expand our dry etching capabilities in 2017 we got an irresistible offer on a twin Pegasus system with cassette to cassette vacuum robot from a commerciel fab. The twin Pegasus system (called Pegasus 3 and 4) is installed at the old cluster 2 location in cleanroom C1 and will run only 6" wafers. Pegasus 3 is the 6" silicon etch work horse and Pegasus 4 will be converted (adding extra process gases) into a 6" dielectric etch tool that will supplement/replace the AOE. As of April 2020, we are still waiting for spare parts for the gas installation. | ||
This page was originally intended as a regular one-machine page (the Pegasus page). However, as of 2018 with several tools, the page will serve as common page for all of our Pegasi | This page was originally intended as a regular one-machine page (the Pegasus 1 page). However, as of 2018 with several tools, the page will serve as common page for all of our Pegasi with subpages for each tool. | ||
{| | {| | ||
Revision as of 09:25, 26 March 2020
Feedback to this page: click here
The DRIE Pegasus tools at DTU Nanolab
In 2010 DTU Nanolab acquired DRIE-Pegasus 1 (at the time called Danchip and DRIE-Pegasus, respectively). As a state-of-the-art etch tool with excellent performance and great flexibility, it grew immensely popular and by 2015 it was apparent that we needed yet another tool to cope with the demand. Therefore, in 2016 Pegasus 2 was acquired from a closed-down lab in Morocco and installed next to Pegasus 1.
Looking to expand our dry etching capabilities in 2017 we got an irresistible offer on a twin Pegasus system with cassette to cassette vacuum robot from a commerciel fab. The twin Pegasus system (called Pegasus 3 and 4) is installed at the old cluster 2 location in cleanroom C1 and will run only 6" wafers. Pegasus 3 is the 6" silicon etch work horse and Pegasus 4 will be converted (adding extra process gases) into a 6" dielectric etch tool that will supplement/replace the AOE. As of April 2020, we are still waiting for spare parts for the gas installation.
This page was originally intended as a regular one-machine page (the Pegasus 1 page). However, as of 2018 with several tools, the page will serve as common page for all of our Pegasi with subpages for each tool.
The Bosch process
The DRIE Pegasus tools are state-of-art silicon dry etchers that offer outstanding performance in terms of etch rate, uniformity etc. They use the so-called Bosch process to achieve excellent control of the etched features. Click HERE for more fundamental information of the system. As of 2017, completing the Dry Etch TPT course is mandatory for all new users. On the TPT web page you will find a version of the latest lecture slides - here you will find information as well.
Links to the individual pages for the Pegasi
- DRIE-Pegasus 1
- DRIE-Pegasus 2
- DRIE-Pegasus 3 - installation in progress
- DRIE-Pegasus 4 - installation in progress
| Equipment | DRIE-Pegasus 1 | DRIE-Pegasus 2 | DRIE-Pegasus 3 | DRIE-Pegasus 4 | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Purpose | Primary |
|
|
|
| ||||||||
| Alternative |
|
|
|
| |||||||||
| Performance | Etch rates |
|
|
|
| ||||||||
| Uniformity |
|
|
|
| |||||||||
| Process parameter range | RF powers |
|
|
|
| ||||||||
| Gas flows |
|
|
|
| |||||||||
| Pressure and temperature |
|
|
|
| |||||||||
| Process options |
|
|
|
| |||||||||
| Substrates | Sizes |
|
|
|
| ||||||||
| Loading |
|
|
| ||||||||||
| Allowed materials |
|
|
|
| |||||||||
| Possible masking materials |
|
|
|
| |||||||||
Process information
SPTS process notation
Describing a process recipe on the Pegasus may sometimes be difficult because of the great flexibility of the instrument. A compact and precise notation is therefore required for the recipes. Click HERE to find a short description of the official SPTS notation.
Hardware changes
A few hardware modifications have been made on the Pegasus 1 since it was installed in 2010. The changes are listed in the table below under hardware options.
| DRIE-Pegasus 1 | DRIE-Pegasus 2 | DRIE-Pegasus 3 | DRIE-Pegasus 4 | |
|---|---|---|---|---|
| Manufactured | 2010 | 2010 | ? | ? |
| Serial | MP0636 | MP0641 | CP0170 | CP0171 |
| Electrode size | 4" | 6" | 6" | 6" |
| Hardware options | ? | ? |
General Pegasus information
Wafer bonding
To find information on how to bond wafers or chips to a carrier wafer, click HERE.
Characterisation of etched trenches
The trenches in deep silicon trenches can be characterized in many ways. Being able to compare processes requires that a set of common measurements and calculations must be established. Click HERE to find more information about the parameters used on the DRIE-Pegasus process development.