Specific Process Knowledge/Back-end processing/Hot Embosser: Difference between revisions
Appearance
| Line 71: | Line 71: | ||
| style="background:LightGrey; color:black"|Allowed materials | | style="background:LightGrey; color:black"|Allowed materials | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* | *PMMA | ||
* | *TOPAS 5013-L10 | ||
*TOPAS 8007 | |||
*PC | |||
*PP | |||
*PCL | |||
*SU8 | |||
*Graphene | |||
*Metals (Al,Ni....) | |||
*For other materials contact for machine responsible personel | |||
|- | |- | ||
|} | |} | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 12:40, 26 February 2020
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Name of equipment
Write a short description of the equipment(s).
The user manual(s), quality control procedure(s) and results, user APV(s), technical information and contact information can be found in LabManager:
Process information
Link to process pages - e.g. one page for each material
Example:
| Equipment | Equipment 1 | |
|---|---|---|
| Purpose |
| |
| Performance | Press Plates Temperature |
|
| Press Plates Pressure |
| |
| Process parameter range | Temperature |
|
| Pressure |
| |
| Substrates | Batch size |
|
| Allowed materials |
| |