== BCB Curing Oven == | == BCB Curing Oven == | ||
[[image:BCB oven.jpeg|350x350px|right|thumb|The BCB Curing Oven. Positioned in | [[image:BCB oven.jpeg|350x350px|right|thumb|The BCB Curing Oven. Positioned in cleanroom A-4]] | ||
The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of some metals in a nitrogen atmosphere. | The BCB Curing Oven is mainly used for curing of BCB (bisbenzocyclobutene) and for alloying of some metals in a nitrogen atmosphere. | ||