Specific Process Knowledge/Thermal Process/Dope with Phosphorus: Difference between revisions
Appearance
New page: The furnace A4 phosphorus predep can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers. |
No edit summary |
||
| Line 1: | Line 1: | ||
The furnace A4 phosphorus predep can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers. | The furnace A4 phosphorus predep(N-predep) can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers. | ||
Revision as of 10:54, 26 January 2009
The furnace A4 phosphorus predep(N-predep) can be used to predeposit silicon wafers with phosphor. The silicon wafers are positioned in a quarts boat. Phosphor is predeposited in the silicon wafers.