*[[/A4 Phosphor Pre-dep furnace|Phosphorus Predep furnace (A4)]] - ''For pre-deposition (doping) of phosphorus on Si wafers'' | *[[/A4 Phosphor Pre-dep furnace|Phosphorus Predep furnace (A4)]] - ''For pre-deposition (doping) of phosphorus on Si wafers'' | ||
*[[/C1 Furnace Anneal-oxide|Anneal-oxide furnace(C1)]] - ''For oxidation and annealing of 100 mm and 150 mm wafers'' | *[[/C1 Furnace Anneal-oxide|Anneal-oxide furnace(C1)]] - ''For oxidation and annealing of 100 mm and 150 mm wafers'' | ||
*[[/C2 Furnace III-V oxidation furnace(C2)]] - ''For oxidation of Al<sub>x</sub>GaAs layers.'' | |||
*[[/C3 Anneal-bond furnace|Anneal-bond furnace (C3)]] - ''For oxidation and annealing of bonded wafers'' | *[[/C3 Anneal-bond furnace|Anneal-bond furnace (C3)]] - ''For oxidation and annealing of bonded wafers'' | ||
*[[/C4 Aluminium Anneal furnace|Aluminium Anneal furnace (C4)]] - ''For annealing of wafers containing aluminium, Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> '' | *[[/C4 Aluminium Anneal furnace|Aluminium Anneal furnace (C4)]] - ''For annealing of wafers containing aluminium, Al<sub>2</sub>O<sub>3</sub> and TiO<sub>2</sub> '' | ||
*[[/Furnace Noble|Noble furnace]] - ''For annealing and oxidation of non-clean wafers'' | *[[/Furnace Noble|Noble furnace]] - ''For annealing and oxidation of non-clean wafers'' | ||
*[[/Furnace APOX|APOX furnace]] - ''For growing of very thick oxide layers'' | *[[/Furnace APOX|APOX furnace]] - ''For growing of very thick oxide layers'' -<span style="color:Red"> (Decommissioned)</span> | ||
*[[/Jipelec RTP|Jipelec RTP]] - ''For rapid thermal annealing of III-V materials and Si based materials'' | *[[/Jipelec RTP|Jipelec RTP]] - ''For rapid thermal annealing of III-V materials and Si based materials'' | ||
*[[/BCB Curing Oven|BCB Curing oven]] - ''For resist curing and metal alloying'' | *[[/BCB Curing Oven|BCB Curing oven]] - ''For resist curing and metal alloying'' | ||
*[[/Furnace: Multipurpose annealing |Furnace: Multipurpose annealing ]] - ''For annealing, oxidation and resist pyrolysis'' | *[[/Furnace: Multipurpose annealing |Furnace: Multipurpose annealing ]] - ''For annealing, oxidation and resist pyrolysis'' | ||
*[[/Resist Pyrolysis Furnace|Resist Pyrolysis furnace]] - ''For pyrolysis of different resist layers'' | *[[/Resist Pyrolysis Furnace|Resist Pyrolysis furnace]] - ''For pyrolysis of different resist layers'' | ||
*[[/D4 III-V Oven|III-V Oven (D4)]] - ''For oxidation of Al<sub>x</sub>GaAs layers.'' | *[[/D4 III-V Oven|III-V Oven (D4)]] - ''For oxidation of Al<sub>x</sub>GaAs layers.'' -<span style="color:Red"> (Decommissioned)</span> | ||
Revision as of 14:17, 14 August 2019
Feedback to this page: click here
Choose a process type
- Oxidation - Grow a thermal oxide on silicon
- Annealing
- Doping with Boron
- Doping with Phosphorus
Choose an equipment to use
- Boron Drive-in + Predep furnace (A1) - For oxidation and annealing of Si wafers, and for boron pre-deposition (doping) and for drive-in afterwards
- Gate Oxide furnace (A2) - For gate oxide growing on new wafers
- Phosphorus Drive-in furnace (A3) - For oxidation and annealing of Si wafers and for drive-in after phosphorus pre-dep
- Phosphorus Predep furnace (A4) - For pre-deposition (doping) of phosphorus on Si wafers
- Anneal-oxide furnace(C1) - For oxidation and annealing of 100 mm and 150 mm wafers
- /C2 Furnace III-V oxidation furnace(C2) - For oxidation of AlxGaAs layers.
- Anneal-bond furnace (C3) - For oxidation and annealing of bonded wafers
- Aluminium Anneal furnace (C4) - For annealing of wafers containing aluminium, Al2O3 and TiO2
- Noble furnace - For annealing and oxidation of non-clean wafers
- APOX furnace - For growing of very thick oxide layers - (Decommissioned)
- Jipelec RTP - For rapid thermal annealing of III-V materials and Si based materials
- BCB Curing oven - For resist curing and metal alloying
- Furnace: Multipurpose annealing - For annealing, oxidation and resist pyrolysis
- Resist Pyrolysis furnace - For pyrolysis of different resist layers
- III-V Oven (D4) - For oxidation of AlxGaAs layers. - (Decommissioned)