Jump to content

Specific Process Knowledge/Thin film deposition/Deposition of Silicon: Difference between revisions

From LabAdviser
Reet (talk | contribs)
added e-beam at top of page as it is in the comparison table
Bghe (talk | contribs)
No edit summary
Line 15: Line 15:
==Deposition of Silicon using sputter deposition technique==
==Deposition of Silicon using sputter deposition technique==


At DANCHIP you can also deposit silicon the using Wordentec, the Lesker Sputter system or the IBE Ionfab300 sputter systems. One of the advantages here is that you can deposit on any material you like.  
At Nanolab you can also deposit silicon the using Wordentec, the Lesker Sputter system or the IBE Ionfab300 sputter systems. One of the advantages here is that you can deposit on any material you like.  


* [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBSD of Si|Si deposition in IBE⁄IBSD Ionfab300]]  
* [[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBSD of Si|Si deposition in IBE⁄IBSD Ionfab300]]  
* [[Specific Process Knowledge/Thin film deposition/Si sputter in Wordentec|Si sputter in Wordentec]]
 
==Deposition of Silicon using PECVD==
 
At Nanolab you can also deposit silicon the using PECVD. The deposition temperature is 300 <sup>o</sup>C. 
 
* [[/Si deposition using PECVD|Si deposition using PECVD3]]


==Comparison of the methods for deposition of Silicon==
==Comparison of the methods for deposition of Silicon==

Revision as of 12:53, 27 June 2019

Feedback to this page: click here


PolySilicon can be deposited in several Danchip tools. It can be sputtered, e-beam evaporated or be deposited in the PolySilicon furnaces. In the chart below you can compare the different deposition methods:


Deposition of PolySilicon using LPCVD

Danchip has two furnaces for deposition of LPCVD (Low Chemical Vapour Deposition) polysilicon: A 6" furnace (installed in 2011) for deposition of standard polySi, amorphous polySi and boron doped polySi on 100 mm or 150 mm wafers and a 4" furnace (installed in 1995) for deposition of standard polySi, amorphous polySi, boron- and phosphorous doped polySi on 100 mm wafers. In LabManager the two furnaces are named "Furnace: LPCVD Poly-Si (4") (B4)" and "Furnace: LPCVD Poly-Si (6") (E2)", respectively.


Deposition of Silicon using sputter deposition technique

At Nanolab you can also deposit silicon the using Wordentec, the Lesker Sputter system or the IBE Ionfab300 sputter systems. One of the advantages here is that you can deposit on any material you like.

Deposition of Silicon using PECVD

At Nanolab you can also deposit silicon the using PECVD. The deposition temperature is 300 oC.

Comparison of the methods for deposition of Silicon

4" and 6" Furnace PolySi (Furnace LPCVD PolySi) Sputter (Wordentec) Sputter (IBE/IBSD Ionfab 300) Sputter (Lesker) E-beam evaporation (III-V Dielectric evaporator)
General description LPCVD (low pressure cheimical vapour deposition) of polysilicon Sputter deposition of Si. Ion beam sputter deposition of Si. Sputter deposition of Si. E-beam evaporation of Si.
Doping facility Can be doped with boron or phosphorus during deposition None None None None
Pre-clean New wafers can go directly into the furnace. Processed wafers have to be RCA cleaned RF Ar clean None RF Ar clean  
Layer thickness ~50Å to 2µm, if thicker layers are needed please ask the furnace team. 10Å to about 3000Å No defined limits 10Å to 2500Å
Deposition rate
  • undoped, boron doped:~100Å/min
  • Phospher doped:~20Å/min

In the order of 1 Å/s, but dependendt on process parameters. See more here.

About 5 nm/min. See more here. Depends on process parameters, roughly 1 Å/s. 1Å/s to 5Å/s (see below).
Process temperature 560 oC (amorph) and 620 oC (poly) ? Platen: 5-60 oC Wafers can be heated to 100-200°C 20-250 oC
Step coverage Good . Not known Poor
Adhesion Good for fused silica, silicon oxide, silicon nitride, silicon . Not tested    
Batch size
  • 1-30 wafers (4" furnace)
  • 1-25 wafes (6" furnace)
  • 24x 2" wafers or
  • 6x 4" wafers or
  • 6x 6" wafers
  • Several small samples mounted with capton tape
  • 1x 50 mm wafer
  • 1x 100 mm wafer
  • 1x 150 mm wafer
  • 1x 200 mm wafer
  • Up to 1x6" wafers
  • smaller pieces
  • 2"
  • chips
Allowed substrates
  • Silicon wafers (new or RCA cleaned)
    • with layers of silicon oxide or silicon (oxy)nitride
    • from the A, B and E stack furnaces
  • Quartz/fused silica wafers (RCA cleaned)
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
  • Same materials as on the allowed materials below
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
  • Silicon wafers
  • Quartz wafers
  • Pyrex wafers
Allowed material Only those above (under allowed substrates).
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar
  • SU-8
  • Metals
  • Silicon, silicon oxides, silicon nitrides
  • Metals from the +list
  • Metals from the -list
  • Alloys from the above list
  • Stainless steel
  • Glass
  • III-V materials
  • Resists
  • Polymers
  • Capton tape
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • Metals
  • III-V materials
  • Silicon wafers
  • Resists
Comment The system is used both for IBSD and IBE. Si deposition can only be performed when it is set up for IBSD.