Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/3scanned: Difference between revisions
Appearance
No edit summary |
|||
| Line 11: | Line 11: | ||
So far we did not add any constraints at all. That means the Al2p spin orbit doublet is free to move anywhere to find a minimum error. | So far we did not add any constraints at all. That means the Al2p spin orbit doublet is free to move anywhere to find a minimum error. | ||
Scrolling through the etch levels (seen in the bottom of the image below slightly to the right) one can see that the fitting is good. There is some energy shifts but we will ignore that for now. | Scrolling through the etch levels (seen in the bottom of the image below slightly to the right) one can see that the fitting is good. There is some energy shifts around etch levels 22-24 but we will ignore that for now. Whether caused by actual chemical shifts (the appearance of intermediate oxidation states of Al2p that causes the spectrum to shift) or poor energy calibration is too soon to say. The O1s peak will probably hold some clues about this. | ||
[[File:ALD sandwidh Al2p.gif]] | [[File:ALD sandwidh Al2p.gif]] | ||
== The Hf4f peak == | |||
The Hf4f peak is fitted next. Maximize the peak and click 'Peak Fit'. | |||
[[File:ALD-Sandwich-42.gif]] | |||
Add two doublets that will be labelled 'Oxide' and 'Reduced'. | |||