=Processing of high resolution spectra =
=Processing of high resolution scanned spectra =
 
The analysis is continued from [[Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/2Survey|'''here''']].
The analysis is continued from [[Specific Process Knowledge/Characterization/XPS/Processing/ALDSandwich1/2Survey|'''here''']].
We start with the Al2p peak. Below is shown the etch level 23. Click 'Peak Fit' and select and Al2p doublet (''Not 'Add Single Peak' '')
[[File:ALD-Sandwich-40.jpp|700px]]

Revision as of 15:46, 16 October 2018

Processing of high resolution scanned spectra

The analysis is continued from here.

We start with the Al2p peak. Below is shown the etch level 23. Click 'Peak Fit' and select and Al2p doublet (Not 'Add Single Peak' )

File:ALD-Sandwich-40.jpp