Jump to content

Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions

Choi (talk | contribs)
Choi (talk | contribs)
Line 6: Line 6:
[[Category: Etch (Wet) bath|Aluminium]]
[[Category: Etch (Wet) bath|Aluminium]]


Ething of Aluminium can be done either wet or dry. For wet etching please see below on this page. Dry etching can be done either with the [[Specific Process Knowledge/Etch/ICP Metal Etcher|ICP Metal Etch]] using Chlorine chemistry or with [[Specific Process Knowledge/Etch/IBE/IBSD Ionfab 300|IBE]] by sputtering with Ar ions.
Wet ething of aluminium can be done using many different acids and bases. Using dilute phosphoric acid gives reasonably good control and compatibility with photoresists. Etching with dilute phosphoric acid is suitable for etching pure aluminium. If the aluminium is alloyed with other metals, other etchants may be better suited. Previously, aluminium with 1,5% silicon was used at DTU Danchip. This alloy is no longer in use at DTU Danchip but a suitable etchant (PES) for this alloy is included below.


=Wet Aluminium Etch=
=Wet Aluminium Etch=