*0-1000 <sup>o</sup>C | *0-1000 <sup>o</sup>C | ||
*III-V materials only to 450 <sup>o</sup>C | |||
*Temperature ramp up to 300 <sup>o</sup>C/min | *Temperature ramp up to 300 <sup>o</sup>C/min | ||
|- | |- | ||
|style="background:LightGrey; color:black"|Process pressure | |style="background:LightGrey; color:black"|Process pressure | ||
Revision as of 11:31, 14 November 2016
Feedback to this page: click here
Jipelec - Rapid Thermal Processing

The Jipelec is a rapid thermal processing (RTP) oven. It is be used for fast and well-controlled annealing or alloying of samples. It is possible to use either a thermocouple or a pyrometer to control the temperature (of the sample carrier).
The user manual, technical information and contact information can be found in LabManager:
| Purpose | RTP annealing | |
|---|---|---|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gasses on the system |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
A silicon carrier wafer with 1 µm oxide is always need (except for III-V materials)
|