A3 Furnace phosphorus drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing and for drive-in of phosphor after a pre-deposition of | A3 Furnace phosphorus drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing and for drive-in of phosphor after a pre-deposition of phosphor in the A4 Furnace phosphorus pre-dep. It can also be used for drive in of phosphor which has been ion implanted. | ||
This furnace is the third furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team. | This furnace is the third furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team. | ||
<br clear="all" /> | <br clear="all" /> | ||
==Process knowledge== | |||
*Phosphorus drive-in: look at the [[Process Knowledge/Thermal Process/Dope with Phosphorus|Dope with Phosphorus]] page | |||
*Oxidation: look at the [[Specific Process Knowledge/Thermal Process/Oxidation|Oxidation]] page | |||
*Annealing: look at the [[Specific Process Knowledge/Thermal Process/Annealing|Annealing]] page | |||
==A rough overview of the performance of the phosphorus drive-in furnace and some process related parameters== | ==A rough overview of the performance of the phosphorus drive-in furnace and some process related parameters== | ||
Revision as of 15:45, 26 February 2008
A3 Furnace Phosphorus drive-in
A3 Furnace phosphorus drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing and for drive-in of phosphor after a pre-deposition of phosphor in the A4 Furnace phosphorus pre-dep. It can also be used for drive in of phosphor which has been ion implanted.
This furnace is the third furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team.
Process knowledge
- Phosphorus drive-in: look at the Dope with Phosphorus page
- Oxidation: look at the Oxidation page
- Annealing: look at the Annealing page
| Purpose | Drive-in of phosphor, oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| . | Process pressure |
|
| . | Gas flows |
|
| Substrates | Batch size |
|
| . | Substrate material allowed |
|