Specific Process Knowledge/Lithography/Coaters/Spin Coater: RCD8 processing: Difference between revisions

Taran (talk | contribs)
Taran (talk | contribs)
Line 46: Line 46:
[[Image:RCD8 SU-8 2075.jpg|300x300px|thumb|right|Spin curve for SU-8 2075]]
[[Image:RCD8 SU-8 2075.jpg|300x300px|thumb|right|Spin curve for SU-8 2075]]
[[Image:RCD8 SU-8 2075 Gyrset.jpg|300x300px|thumb|right|Spin curve for SU-8 2075 using Gyrset]]
[[Image:RCD8 SU-8 2075 Gyrset.jpg|300x300px|thumb|right|Spin curve for SU-8 2075 using Gyrset]]
Spin coating of SU-8 2075 on Spin Coater: RCD8 is...
Spin coating of SU-8 2075 on Spin Coater: RCD8 using automatic dispense is...


''Recipe names, process parameters, and test results:''
''Recipe names, process parameters, and test results:''