III-V Oven (D4)
The III-V Oven (D4) is used for wet thermal oxidation of III-V devices, for instance for lateral oxidation of thin AlGaAs layers to defined apertures in light-limiting diodes.
The furnace is an old Tempress horizontal furnace. The quartz boat is loaded manually into the furnace by use of a push rod. The furnace is cooled down to room temperature when it is not being used.
Before use, devices have to be cleaned. A short BHF dip can be used to remove any native oxide which can be difficult to penetrate by a wet thermal oxidation.
Please check the cross contamination information in LabManager before you use the furnace.
The user manual and contact information can be found in LabManager:
Process knowledge
Purpose |
| |
---|---|---|
Performance | Lateral oxidation rate |
|
Process parameter range | Process temperature |
|
Process pressure |
| |
Gasses on the system |
| |
Substrates | Batch size |
|
Substrate materials allowed |
|