Specific Process Knowledge/Characterization/AFM: Atomic Force Microscopy/AFM Icon Acceptance: Difference between revisions

Bghe (talk | contribs)
Bghe (talk | contribs)
Line 126: Line 126:
Scan size 0.01nm <br>
Scan size 0.01nm <br>
We saw some 50Hz noise (electrical - or maybe pumps): Rq 15 pm (specs 35pm) <br>
We saw some 50Hz noise (electrical - or maybe pumps): Rq 15 pm (specs 35pm) <br>
[[File:SensorNoise.jpg|thumb|left|400px]] <br>
[[File:SensorNoise.jpg|thumb|left|400px]] <br clear="all" />


====System noise====
====System noise====