Specific Process Knowledge/Lithography/LiftOff: Difference between revisions
Appearance
| Line 35: | Line 35: | ||
|style="background:LightGrey; color:black"|Ultrasonic agitation | |style="background:LightGrey; color:black"|Ultrasonic agitation | ||
|style="background:WhiteSmoke; color:black" align="center"| | |style="background:WhiteSmoke; color:black" align="center"| | ||
Continuous | |||
|style="background:WhiteSmoke; color:black" align="center"| | |style="background:WhiteSmoke; color:black" align="center"| | ||
Continuous or pulsed | |||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | ||
Revision as of 16:24, 5 March 2014
Feedback to this page: click here
Comparing Lift-off equipment
| Equipment | Lift-off Wet Bench | Lift-off (4", 6") | |
|---|---|---|---|
| Purpose |
|
| |
| Bath chemical |
Acetone |
NMP (Remover 1165) | |
| Process parameters | Process temperature |
Room temperature |
Heating of the bath is possible. The heating has been limited to 37°C |
| Ultrasonic agitation |
Continuous |
Continuous or pulsed | |
| Substrates | Substrate size |
|
|
| Allowed materials |
All cleanroom materials |
All cleanroom materials | |
| Batch |
1 - 25 |
1 - 8 | |
Lift-off Wet Bench

This bench is only for wafers with metal!
Here are the main rules for lift-off bench use:
- Place the wafers in a dedicated wafer holder.
- Put the holder in the acetone and start the ultrasound. The strip off time is depending of resist thickness.
- Rinse your wafers for 4-5 min. in running water after stripping.
Find more info about the lift-off process here: Specific Process Knowledge/Photolithography/AZ5214E standard resist - reverse process