| Steel (50µm)
| Red(532nm/255mm)
| 200 kHz
| 100%
| 0,55 W
| 50 mm/s
| 1 burst
| 0
| 22
|
|
| [[media:TB_532nm_255mm_cutting_steel_50um.xls|Cutting steel 50µm]]
| Cutting through. Dicing shrim for Injection molder.
|-
|}
|}