| 1  
| 1  
| N/A
| N/A
| [[media:Cutting_Ni_320µm.xls|Cutting Ni 320µm parameters]]
| [[media:TB_532nm_255mm_cutting_Ni_320um.xls|Cutting Ni 320µm parameters]]
| Cutting through only blue tape left  
| Cutting through only blue tape left  
|-
|-