|Recipe name  
|Recipe name  
|SiH4 flow [sccm]
|SiH4 flow [sccm]
|N<math>_2</math>O flow [sccm]
|N<sub>2</sub>O flow [sccm]
|N2 flow [sccm]
|N2 flow [sccm]
|B2H6 flow [sccm]
|B2H6 flow [sccm]