=Fabrication of Hyperbolic Metamaterials by ALD: AZO Gratings=
=Fabrication of Hyperbolic Metamaterials by ALD: AZO Pillars=


The fabrication and characterization described below were conducted in <b>2013-2016 by Evgeniy Shkondin, DTU Nanolab</b>.<br>
The fabrication and characterization described below were conducted in <b>2013-2016 by Evgeniy Shkondin, DTU Nanolab</b>.<br>