Specific Process Knowledge/Thin film deposition/Deposition of Chromium/Thermal evaporation of Cr in Thermal evaporator: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
Line 230: Line 230:
</gallery>
</gallery>


The following model is selected for XRR fitting: Native chromium oxide, bulk chromium layer, native silicon oxide, and the bulk silicon substrate.
The following model is selected for XRR fitting: Native chromium oxide, bulk chromium layer, native silicon oxide, and the bulk silicon substrate. fitting result presented in the table.