Tempress) based on SiH<sub>4</sub> at 560 °C. This procedure enables the preparation of home-made silicon-on-insulator (SOI) substrates. | Tempress) based on SiH<sub>4</sub> at 560 °C. This procedure enables the preparation of home-made silicon-on-insulator (SOI) substrates. | ||
The main steps in the fabrication of pillars and tubes are shown in Fig 1. Initially, silicon holes were etched in SOI wafers by deep-UV lithography and DRIE (Fig. 1(a)-1(c)). The holes were arranged in a square lattice with the pitch of 400 nm. The template was then filled with an ALD D25 AZO coating (Fig. 1(d)) at 250 °C. The thickness of the deposited AZO depends on the desired output. An entire filling would result in the formation of pillars, while partial deposition leads to fabrication of hollow tubes. After removal of the top parts by Ar+ ion sputtering (Fig. 1(e)), the silicon core between the ALD coated holes was etched away during the last step. Figure 1(f) represents the final structures. Fabrication output is shown in Fig. 2. Each process step was carefully analyzed using cross-sectional SEM imaging (see Figs. 3 and 4 for tubes | The main steps in the fabrication of pillars and tubes are shown in Fig 1. Initially, silicon holes were etched in SOI wafers by deep-UV lithography and DRIE (Fig. 1(a)-1(c)). The holes were arranged in a square lattice with the pitch of 400 nm. The template was then filled with an ALD D25 AZO coating (Fig. 1(d)) at 250 °C. The thickness of the deposited AZO depends on the desired output. An entire filling would result in the formation of pillars, while partial deposition leads to fabrication of hollow tubes. After removal of the top parts by Ar+ ion sputtering (Fig. 1(e)), the silicon core between the ALD coated holes was etched away during the last step. Figure 1(f) represents the final structures. Fabrication output is shown in Fig. 2. Each process step was carefully analyzed using cross-sectional SEM imaging (see Figs. 3 and 4 for pillars and tubes fabrication, respectively). | ||
<br clear="all" /> | <br clear="all" /> | ||
| Line 14: | Line 14: | ||
<gallery caption="" widths="500px" heights="600px" perrow="2"> | <gallery caption="" widths="500px" heights="600px" perrow="2"> | ||
image: | image:AZO_pillars_fab_supplementary_eves.jpg| Figure 3. SEM verification for each fabrication step of pillars production. Left side shows cross-sectional images and right side of the Figure shows the top view of the structures. | ||
image: | image:AZO_tubes_fab_supplementary_eves.jpg| Figure 4. SEM verfication for each fabrication step of tube production. Left side shows cross-sectional images and right side of the Figure shows the top view of the structures. | ||