Specific Process Knowledge/Thin film deposition/Deposition of Silicon Oxide: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Silicon_Oxide click here]''' | |||
Deposition of Silicon Oxide can be done with either LPCVD, PECVD or by sputter technique. You can also make a silicon oxide layer by growing a [[Specific Process Knowledge/Thermal Process/Oxidation|thermal oxide]] in a hot furnace but that requires a silicon surface as a starting point. | Deposition of Silicon Oxide can be done with either LPCVD, PECVD or by sputter technique. You can also make a silicon oxide layer by growing a [[Specific Process Knowledge/Thermal Process/Oxidation|thermal oxide]] in a hot furnace but that requires a silicon surface as a starting point. | ||