Revision as of 10:44, 24 April 2013

3rd Level - Material/Methode

Feedback to this page: click here


Choose material to deposit

Dielectrica

Metals/elements

Period/Group

IVB VB VIB VIIIB IB IIIA IVA
3 . . . . . 13 Al Aluminium 14 Si Silicon
4 22 Ti Titanium . 24 Cr Chromium 28 Ni Nickel 29 Cu Copper . 32 Ge Germanium
5 . . 42 Mo Molybdenum 46 Pd Palladium 47 Ag Silver . 50 Sn Tin
6 . 73 Ta Tantalum 74 W Tungsten 78 Pt Platinum 79 Au Gold . .

Alloys


Polymers

  • SU8
  • Antistiction coating
  • Topas
  • PMMA

Choose deposition equipment