*[[/Jipelec RTP|Jipelec RTP]] - ''For Rapid Thermal Anneal of III-V materials and Silicon based material'' | *[[/Jipelec RTP|Jipelec RTP]] - ''For Rapid Thermal Anneal of III-V materials and Silicon based material'' | ||
*[[/BCB Curing Oven|BCB Curing Oven]] - ''...'' | *[[/BCB Curing Oven|BCB Curing Oven]] - ''...'' | ||
*[[/Resist Pyrolysis Furnace|Resist Pyrolysis Furnace]] - ''For | *[[/Resist Pyrolysis Furnace|Resist Pyrolysis Furnace]] - ''For pyrolysis of different resist layers'' | ||
The Resist Pyrolysis Furnace is used for resist pyrolysis, where samples with different resist layers are heated up to maximum 1000°C in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample | The Resist Pyrolysis Furnace is used for resist pyrolysis, where samples with different resist layers are heated up to maximum 1000°C in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample | ||
Revision as of 15:10, 30 November 2012
Choose a process type
- Oxidation - grow a thermal oxide
- Annealing
- Dope with Boron
- Dope with Phosphorus
Choose an equipment to use
- A1 Bor Drive-in furnace - For oxidation of new wafers and for drive-in of Boron pre-dep
- A2 Bor Pre-dep furnace - Dope with Boron: For predeposition of Boron on wafers
- A3 Phosphor Drive-in furnace - For oxidation of new wafers and for drive in of Phosphorus pre-dep
- A4 Phosphor Pre-dep furnace - Dope with Phosphorus: For predeposition of Phosphorus on wafers
- C1 Furnace Anneal-oxide - For oxidation and annealing, up to 6" wafer
- C2 Gate Oxide furnace - For growing of Gate Oxide on new wafers
- C3 Anneal-bond furnace - For annealing and annealing of bonded wafers
- C4 Aluminium Anneal furnace - For oxidation and annealing of wafers containing Aluminium
- Furnace Noble - For non-clean annealing and oxidation
- Furnace APOX - Furnace for growing very thick oxide
- Jipelec RTP - For Rapid Thermal Anneal of III-V materials and Silicon based material
- BCB Curing Oven - ...
- Resist Pyrolysis Furnace - For pyrolysis of different resist layers
The Resist Pyrolysis Furnace is used for resist pyrolysis, where samples with different resist layers are heated up to maximum 1000°C in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample