== The standard processes: Processes  A, B, C, D and SOI ==
The instrument was accepted on the basis of the performance of 5 processes. These standard processes are described below.
{| border="2" cellpadding="2" cellspacing="1" style="text-align:center;"
|+ '''Most commonly used processes on DRIE-Pegasus'''
|-
! rowspan="2" | Process name
! rowspan="2" | Type
! rowspan="2" | Purpose
! colspan="4" | Conditions during original runs
! rowspan="2" | Best usage
|-
! width="120" | Feature
! width="120" | Mask material
! width="120" | Etch load
! width="120" | Comments
|-
! [[Specific Process Knowledge/Etch/DRIE-Pegasus/processA|Process A]]
| Bosch
| Fast etch
| 80 µm trench
| Photo resist
| 12-13 % on 6" wafer
|   
|   
|-
! [[Specific Process Knowledge/Etch/DRIE-Pegasus/processB|Process B]]
| Bosch
| Fast etch
| 30 µm diameter via
| Photo resist
| 12-13 % on 6" wafer
|
|
|-
|}


=== Process A ===
=== Process A ===

Revision as of 12:49, 26 November 2012

The DRIE Pegasus at Danchip

The SPTS Pegasus in the Danchip cleanroom

The Bosch process

The DRIE Pegasus is a state-of-art silicon dry etcher that offers outstanding performance in terms of etch rate, uniformity etc. It uses the so-called Bosch process to achieve excellent control of the etched features. Click here for more fundamental information of the system.

User manuals etc.

The user manual, quality control procedure and the results may all be found on the DRIE-Pegasus LabManager page.

Important information

In August 2011 we introduced a new set of rules regarding the loading of wafers. In you were trained prior to this, you can find more information here.

Acceptance test

The instrument was opened for users in April 2010 when the acceptance test was signed. This was based on the performance of five standard recipes (A, B, C, D and SOI) that are further examined below. The acceptance test report is found here.

Process information

Process notation

Describing a process recipe on the Pegasus may sometimes be difficult because of the great flexibility of the instrument. A compact and precise notation is therefore required for the recipes. Click here to find a short description of the official SPTS notation.

Standard recipes


Process A

Process A is labelled Large trench (80μm wide) 150μm depth. In the acceptance test the process was run on a 150 mm SPTS wafer with 12-13 % etch load.

Process A: Recipe, specifications and results

Process B

Process A is labelled Via (30μm diameter) 100μm depth. In the acceptance test the process was run on a 150 mm SPTS wafer with 12-13 % etch load.

Process B: Recipe, specifications and results

Process C

Process A is labelled Nano silicon etch. In the acceptance test the process was run on a 100 mm Danchip wafer with a test pattern of a series of lines and dots with sizes ranging from 30 nm to 300 nm. The etch load was extremely high, approaching 100 %.

Process C: Recipe, specifications and results

Process D

Process D is labelled Micro stamp etch.

In the acceptance test the process was run on a 100 mm wafer with 50 % etch load.

Process D: Recipe, specifications and results

SOI etch

The SOI etch uses the Low frequency (LF) platen generator to minimize the notching at buried stop layers such as the BOX layer in a SOI wafer.

SOI etch: Recipe, specifications and results

Other processes

Nanoetching

Nanoetch

Wafer thinning

Sloped sidewalls

For injection molding purposes


Processing challenges

Bonded wafers

User manuals

  • The Danchip user manual from LabManager is found >Here<.
  • The user manual provided by SPTS can be found here >HERE<

Hardware information

Hardware Information - Overview.

Hardware Information - Detailed.

The Advantages the Pegasus has over existing Si etchers.

Robot Handling System Information .

Process applications

MEMS in Aerospace.

Bio Medical.

MEMS in Energy.

Nanotechnology.

Packaging Applications.

General Applications.


Further info:

FAQ (Under construction)