=Manual beaker development in fumehood=
=Manual beaker development in fumehood=
Beaker development, in fume hood 09: UV development or fume hood 10: e-beam development, is a fall-back option if you have a process, which is not compatible with the automatic, or semi-automatic, tools. We always recommend using, or at least trying, the automatic and semi-automatic tools, instead of using manual beaker development.
Beaker development, in fume hood 09: UV development or fume hood 10: e-beam development, is a fall-back option if you have a process, which is not compatible with the automatic, or semi-automatic, tools. We always recommend using, or at least trying, the automatic and semi-automatic tools, instead of using manual beaker development.