*[[Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using RIE1 or RIE2|Etch of silicon oxide using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using RIE1 or RIE2|Etch of silicon oxide using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Silicon Nitride/Etch of Silicon Nitride using RIE|Etch of silicon nitride using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Silicon Nitride/Etch of Silicon Nitride using RIE|Etch of silicon nitride using RIE]]
*[[Specific Process Knowledge/Etch/Etching of Polymer/Etch of Photo Resist using RIE|Etch of photo resist using RIE]]
<br clear="all" />
<br clear="all" />
Revision as of 16:24, 20 June 2025
Both RIE's (RIE1 and RIE2) for silicon based etching has been decommissioned.
This information is save because it might be valuable as inspiration for other dry etch systems.
Etching using the dry etch technique RIE (Reactive Ion Etch)
RIE2 (part of Cluster2)- positioned in clean room C-1
We had two RIE's. RIE2 for etching silicon based materials, resist and polymers and one (III-V RIE) for etching III-V materials. Here only RIE2 will be described.
In RIE2 it is allowed to have small amounts of metals exposed to the plasma.
The user manuals, quality control procedures and results, user APVs, technical information and contact information can be found in LabManager: