Feedback to this page: click here
This section is written by DTU Nanolab internal if nothing else is stated.
Mechanical preparation equipment is available for experience users, who know how to use the equipment. Access to the preparation lab is needed. We do not provide training on the equipment.
Cutting
Struers Minitom
Well Precision Diamond Wire Saw
Ultrasonic cutter
Manual - requires login

.
Grinding/Polishing
TechPrep Allied
The MultiPrep™ System enables precise semiautomatic sample preparation of a wide range of materials for microscopic (optical, SEM, FIB, TEM, AFM, etc.) evaluation.
Capabilities include parallel polishing, angle polishing, site-specific polishing or any combination thereof. It provides reproducible results by eliminating inconsistencies between users, regardless of their skill.

Dimple Grinder
Manual - requires login

.
Ion Milling
Fischione NanoMill model 1040
This TEM specimen preparation system is an excellent tool for creating the high-quality thin specimens needed for advanced transmission electron microscopy imaging and analysis. It is ideal for both post-FIB (focused ion beam) processing and the enhancement of conventionally prepared specimens.
Missing equipment
Mini grinder/polisher
Sample preparation processes
Here we collected a few sample preparation processes done at DTU Nanolab building 314/307: