Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency.  
Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency.  

Revision as of 11:26, 8 September 2023

The contents on this page, including all images and pictures, was created by DTU Nanolab staff unless otherwise stated.

Feedback to this page: click here

File:MTP.tif

Micro Transfer Printer


Micro transfer printing is an emerging technique to transfer diverse and non-native components from source substrate to target substrate. Micro transfer printing is best for achieving heterogeneous integration, where micro-components from different sources are picked up by polymer stamp and precisely assembled onto different target substrate such as glass, plastic, ceramic and silicon. This method is known for increasing functionality and improving efficiency.

Micro transfer printer 100 from Xdisplay was installed in year 2022 and placed in cleanroom F-4.

Equipment info in Lab Manager - requires login



Equipment performance and process related parameters

Purpose

Pick and Print

Material handling configuration

Manual

Stage max. travel time (X x Y mm)

300 x 300

Source size (mm)

upto 150

Target size (mm)

upto 150

Alignment accuracy (single post stamp)

<0.5um

Allowed material

All cleanroom materials