Revision as of 12:29, 22 August 2023

Feedback to this page: click here
The content on this page, including all images and pictures, was created by Berit Herstrøm @ DTU Nanolab (BGHE), unless otherwise stated.

Etching of silicon rich nitride (SRN) with recipes developed for SiO2 etching

Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab

Parameter Recipe name: SiO2_res_10 Recipe name: DOE2/Post_II_21
Coil Power [W] 2500 3840
Platen Power [W] 300 300
Platen temperature [oC] 20 20
H2 flow [sccm] 25.6 0
He flow [sccm] 448.7 0
C4F8 flow [sccm] 25.6 30
Pressure [mTorr] 8.8 0.9


Typical results SiO2_res_10 DOE2/Post_II_21
Average etch of SRN on 6" wafer 166 nm/min [+- 17% over a 6" wafer] 142 nm/min [+- 9% over a 6" wafer]
Etch rate of Si3N4 ? ?
Etch rate of SiO2 250 nm/min [+- 3% over a 6" wafer] 306 nm/min [on small piece]
Etch rate in Si ?nm/min ? nm/min
Etch rate of Mir resist ? nm/min ? nm/min

Etch rate uniformity