|Roughness measurement can be done in both Contact, Tapping and ScanAsyst mode. We recommend '''ScanAsyst mode''' because of less chance of (non-uniform) deformation of the sample and less tip wear - and because of ease of use. However it also works fine in tapping mode.
|Roughness measurement can be done in both Contact, Tapping and ScanAsyst mode. We recommend '''ScanAsyst mode''' because of less chance of (non-uniform) deformation of the sample and less tip wear - and because of ease of use. However it also works fine in tapping mode.
|For Topographic measurements with no steep/abrupt steps we also recommend '''Tapping mode''' on most samples. Only on very soft samples (e.g. cells) we recommend ''ScanAsyst'' due to less chance of (non-uniform) deformation of the sample - or if you need QNM data. We mainly recommend '''Tapping mode''' because we experience less problems when the tip end is slightly broken.  
|For Topographic measurements with no steep/abrupt steps we also recommend '''Tapping mode''' on most samples. Only on very soft samples (e.g. cells) we recommend ''ScanAsyst'' due to less chance of (non-uniform) deformation of the sample - or if you need QNM data. We mainly recommend '''Tapping mode''' because we experience less problems when the tip end is slightly broken.  
|For Steep/abrupt steps but no high aspect ratio structures we still recommend '''Tapping mode''' or '''ScanAsyst mode" .  
|For Steep/abrupt steps but no high aspect ratio structures we still recommend '''Tapping mode''' unless you need need QNM data.  
|For High aspect ratio measurements we recommend Tapping mode. We do not have experience with ScanAsyst therefore we recommend '''Tapping mode'''.
|For High aspect ratio measurements we recommend Tapping mode. We do not have experience with ScanAsyst therefore we recommend '''Tapping mode'''.
|For large scan areas where you prioritize to scan fast then you can use '''contact mode'''. Here you can scan with scan rate of up to 2.43 Hz
|For large scan areas where you prioritize to scan fast then you can use '''contact mode'''. Here you can scan with scan rate of up to 2.43 Hz