The 2" coater station is equipped with 1 resist line, as well as 1 syringe line:
The 2" coater station is equipped with 1 resist line, as well as 1 syringe line:
*AR-P 6200.09 (CSAR)
*AR-P 6200.09 (CSAR)
*Syringe, which can be used for various resists (anisole-based or PGMEA-based).
*Syringe, which can be used for various resists (anisole-based or PGMEA-based). ''We currently recommend against using the syringe, as the process setup is quite demanding. Use a manual spin coater instead.''
 


The 4"/6" coater station is equipped with 4 different resists lines:  
The 4"/6" coater station is equipped with 4 different resists lines:  
Line 15: Line 16:
*AZ 4562   
*AZ 4562   


The processes that are available on the system are developed by Nanolab. Upon request, it is possible to establish new processes. Use of the syringe requires special training, and would as a starting point require batches in excess of 20 wafers.
The processes that are available on the system are developed by Nanolab. Upon request, it is possible to establish new processes. Use of the syringe requires special training, and ''requires'' batch processing - it is not for processing a few wafers now and then.


'''[https://www.youtube.com/watch?v=3JhM3rmLVpA Training video]'''