Specific Process Knowledge/Lithography/Descum: Difference between revisions
Appearance
| Line 124: | Line 124: | ||
[[image:descum_graf.jpg|640px|thumb|Descum results plasma asher 2 - recipe 1]] | [[image:descum_graf.jpg|640px|thumb|Descum results plasma asher 2 - recipe 1]] | ||
The user manual(s), quality control procedure(s) and results and contact information can be found in [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=200 LabManager] - '''requires login''' | |||
Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber. | Descum of AZ Mir 701 resist on 100mm silicon wafer. Five wafers were placed vertically in chamber. | ||