The stylus profiler Dektak150 is intended for profile measurements on samples outside the cleanroom. It is located in Packlab in building 347.
The stylus profiler Dektak150 is intended for profile measurements on samples outside the cleanroom. It is located in Packlab in building 347. Packlab is a low-class cleanroom. The Dekta150 is especially well suited for measuring soft samples as it can be adjusted to apply lower force than the other stylus profilers at Nanolab.