Specific Process Knowledge/Thermal Process/E1 Furnace Oxidation (8"): Difference between revisions
Appearance
| Line 65: | Line 65: | ||
*N<sub>2</sub>: 0-10 slm | *N<sub>2</sub>: 0-10 slm | ||
*O<sub>2</sub>: 0-10 slm | *O<sub>2</sub>: 0-10 slm | ||
*Steamer flow : 0- | *Steamer flow : 0-12.5 slm (Standard recipe is set at 9.5 slm ) | ||
|- | |- | ||
!style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | !style="background:silver; color:black" align="center" valign="center" rowspan="2"|Substrates | ||