Line 17: Line 17:
* CMOS camera 4096x4096px resolution with minimum exposure time of 41ms (24fps).<br />
* CMOS camera 4096x4096px resolution with minimum exposure time of 41ms (24fps).<br />
* 15.5x15.5µm<sup>2</sup> pixel size<br />
* 15.5x15.5µm<sup>2</sup> pixel size<br />
<br />


== additional software features in EMplified ==
== additional software features in EMplified ==

Revision as of 08:27, 8 October 2021

Feedback to this page: click here

(content by Jens Kling, September 2021)

THIS PAGE IS UNDER CONSTRUCTION


TVIPS camera and EMplify software

Here you find some information about the TVIPS XF416 camera and some tips and bugs for the EMplify software.


XF416 camera

  • CMOS camera 4096x4096px resolution with minimum exposure time of 41ms (24fps).
  • 15.5x15.5µm2 pixel size


additional software features in EMplified

Tips and bugs in EMplified

Status: October 2021


  • The live view images jumps


  • The acquired image becomes white


  • I can't see anything in the Powerspectrum