Specific Process Knowledge/Thin film deposition/Deposition of Chromium: Difference between revisions
Appearance
| Line 144: | Line 144: | ||
[[/Sputtering of Cr in Wordentec|Sputtering of Cr in Wordentec]] - ''Settings and deposition rates'' | [[/Sputtering of Cr in Wordentec|Sputtering of Cr in Wordentec]] - ''Settings and deposition rates'' | ||
[[/Sputtering of Cr in Sputter System (Lesker)|Sputtering of Cr in Sputter system (Lesker)]] - ''Settings and deposition rates'' | |||
[[/Thermal evaporation of Cr in Thermal evaporator|Thermal evaporation of Cr in Thermal evaporator]] - ''Settings and deposition results'' | [[/Thermal evaporation of Cr in Thermal evaporator|Thermal evaporation of Cr in Thermal evaporator]] - ''Settings and deposition results'' | ||
[[Specific_Process_Knowledge/Thin_film_deposition/Lesker/Stress_dependence_on_sputter_parameters_in_the_Lesker_sputter_system#Cr:_High_tensile_stress|Stress in sputtered Cr films]] - ''Extremely high tensile stress in Cr films deposited at high temperature'' | [[Specific_Process_Knowledge/Thin_film_deposition/Lesker/Stress_dependence_on_sputter_parameters_in_the_Lesker_sputter_system#Cr:_High_tensile_stress|Stress in sputtered Cr films]] - ''Extremely high tensile stress in Cr films deposited at high temperature'' | ||