Specific Process Knowledge/Thin film deposition/thermalevaporator: Difference between revisions
Appearance
| Line 10: | Line 10: | ||
The main purpose of the thermal evaporator is to deposit Al for removing charging of the resist when doing EBL on isolating substrate. | The main purpose of the thermal evaporator is to deposit Al for removing charging of the resist when doing EBL on isolating substrate. | ||
It is not only usable for Al deposition. The thermal evaporator has room for two evaporation sources and thereby the possibility to make thin films of two different metals. At the moment not that many metals have been tested, so right now only Al and Ag can be evaporated. We have attempted to evaporate Au | It is not only usable for Al deposition. The thermal evaporator has room for two evaporation sources and thereby the possibility to make thin films of two different metals. At the moment not that many metals have been tested, so right now only Al and Ag can be evaporated. Cr can also be evapoarated (with very good results), but require a major change in hardware configuration. We have attempted to evaporate Au and Zn but these are not standard processes. If you would like to deposit these or other metals, please talk to the Thin Film group. | ||
Compared to the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]], the thermal evaporator is quicker to use if you only need to deposit on one wafer or on small samples, as it only takes about 15 minutes to pump down the chamber. You can also deposit thicker layers because the throw distance from source to sample is shorter, so the material use is more efficient: In the thermal evaporator, you get up to 200 nm per metal pellet, whereas in the Wordentec you get about 15 nm per pellet. However, the thickness uniformity is better for large samples in the Wordentec also because of the longer distance from source to sample. | Compared to the [[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]], the thermal evaporator is quicker to use if you only need to deposit on one wafer or on small samples, as it only takes about 15 minutes to pump down the chamber. You can also deposit thicker layers because the throw distance from source to sample is shorter, so the material use is more efficient: In the thermal evaporator, you get up to 200 nm per metal pellet, whereas in the Wordentec you get about 15 nm per pellet. However, the thickness uniformity is better for large samples in the Wordentec also because of the longer distance from source to sample. | ||