|ItemName= Available gasses and gas chemistry | |ItemName= Available gasses and gas chemistry | ||
|ItemConfiguration= | |ItemConfiguration=   | ||
* SF<sub>6</sub>: 50 sccm | * SF<sub>6</sub>: 50 sccm | ||
* O2: 50 sccm | * O2: 50 sccm | ||
Revision as of 11:25, 14 December 2020
Feedback to this page: click here
This system is a research tool and not available to the users
If you want to get access to the tool, then talk to professor Henry Jansen
Current setup and rules on Pegasus 2
Click here to access older configurations.
The current configuration is
Access to Pegasus 2 configuration templates
Pegasus 2 configuration table version 1
- Table header: Template:Peg2configheader1
- Table content: Template:Peg2configcontent1
| Item | The currently applied modification | Comments |
|---|---|---|
| Available gasses and gas chemistry |  
|
OnlySF6 and O2 are used for Si, PR, and Cr etch. The rest is only make-up |