Jump to content

Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-3: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Jmli (talk | contribs)
Line 50: Line 50:


  <!-- *[[Specific Process Knowledge/Etch/DRIE-Pegasus/VeeryDeeep| Very deep etching]] -->
  <!-- *[[Specific Process Knowledge/Etch/DRIE-Pegasus/VeeryDeeep| Very deep etching]] -->
=== Advanced Processing - Henri Jansen style ===
* [[Specific Process Knowledge/Etch/DRIE-Pegasus/Etch silicon nanostructures|Etch silicon nanostructures ]]
* [[Specific Process Knowledge/Etch/DRIE-Pegasus/Etch high aspect ratio silicon microstructures|Etch high aspect ratio silicon microstructures ]]
* [[Specific Process Knowledge/Etch/DRIE-Pegasus/Etch 3 dimensional silicon microstructures|Etch 3 dimensional silicon microstructures]]
* [[Specific Process Knowledge/Etch/DRIE-Pegasus/Etch black silicon|Etch black silicon]]
* [[Specific Process Knowledge/Etch/DRIE-Pegasus/Using OES to monitor etch process|Using OES to monitor etch process]]


=== Wafer bonding ===
=== Wafer bonding ===

Revision as of 17:00, 16 November 2020

Feedback to this page: click here


Pegasus 3 - 150mm silicon etching

The tool is ready for user training.

The Pegasus 3 cassette station (left), operator station (center) and support computer with Picoscope process monitoring.


The user manual(s) is available, technical information and contact information can be found in LabManager:

Equipment info in LabManager

Process information

Standard recipes

Hardware changes

Compared to a standard SPTS DRIE Pegasus chamber, the Pegasus 3 has had the same modifications as the Pegasus 1 with the exception of the Claritas EPD system. The changes are listed below.


Other etch processes

More processes, such as for DUV resist, are currently being developed, but they are not quite 'ready for publication' at LabAdviser so please contact Jonas (mailto:jmli@dtu.dk) for more information.



Wafer bonding

To find information on how to bond wafers or chips to a carrier wafer, click here.

Characterisation of etched trenches

Comparing differences in etched trenches requires a set of common parameters for each trench. Click HERE to find more information about the parameters used on the DRIE-Pegasus process development.


Internal Nanolab Process log for Pegasus 3

Process log at Nanolab [1]