=The XRD Powder setup=
=The XRD Powder setup=
[[Image:machine front with on-off button.JPG|right|thumb|300px|The XRD Powder located in the basement of building 346 at Nanolab, Room 904.]]
The "XRD powder" is an Aeris Research edition benchtop X-ray diffractometer from Malvern Panalytical. It is meant for phase analysis of powders, is easy to use, and offers the option of making measurements while heating the sample in a N<sub><sub>2</sub></sub> atmosphere. The setup allows X-ray diffraction measurements in Bragg-Brentano mode (i.e., Theta-2Theta measurements where the incident and diffraction arms of the goniometer are coupled). We have a very limited selection of optics for this instrument, so there is little that the user can adjust.


The "XRD powder" is a benchtop X-ray diffractometer from Panalytical for phase analysis of powders. It is easy to use and offers the option of making measurements while heating the sample in a N<sub><sub>2</sub></sub> atmosphere. The instrument is located in the basement of building 346 at Nanolab, Room 904.  
Please contact the equipment responsible if you would like to mount the special sample holder for heating during the measurement.  
 


'''The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:'''  
'''The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:'''  
Line 10: Line 11:
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=463 XRD Powder in LabManager]
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=463 XRD Powder in LabManager]


==Process information==
*A detailed manual on the Aeris XRD is found on the [https://wiki.iodp.tamu.edu/display/LMUG/Aeris+Advanced+User+Guide|wiki of the International Ocean Discovery Project].
Malvern Panalytical has a large collection of webinars on XRD. You have to register to view them but the amount of email you receive afterwards is modest, so it's worth it in my opinion (Rebecca, July 2022).
*A nice webinar about sample preparation: [https://www.malvernpanalytical.com/en/learn/events-and-training/webinars/W20200604XRD.html|Better XRD data quality with good sample preparation]
*A [https://www.malvernpanalytical.com/en/learn/events-and-training/webinars/W20210330XRD.html|beginner’s tutorial] which also mentions sample preparation about half-way through and explains very briefly some of the issues that can arise from displaced samples, not having a thick enough sample layer, odd sized sample particles, etc.
==Software==
==Software==
After making a measurement, you will need dedicated software for the data export and analysis.
After making a measurement, you will need dedicated software for the data export and analysis.
Line 22: Line 34:
If you are going to make measurements in a heated N<sub><sub>2</sub></sub> atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.
If you are going to make measurements in a heated N<sub><sub>2</sub></sub> atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.


==Measurements==
This setup allows you to make X-ray diffraction measurements in Bragg-Brentano mode (i.e., Theta-2Theta measurements where the incident and diffraction arms of the goniometer are coupled).
We have a very limited selection of optics for this instrument, so there is little that the user can adjust.
It is possible to mount a special sample holder for heating the sample during the measurement. Please contact the equipment responsible to ask about this option.


==Equipment performance and process related parameters==
==Equipment performance and process related parameters==

Revision as of 11:38, 8 July 2022

Feedback to this page: click here

The XRD Powder setup

The XRD Powder located in the basement of building 346 at Nanolab, Room 904.

The "XRD powder" is an Aeris Research edition benchtop X-ray diffractometer from Malvern Panalytical. It is meant for phase analysis of powders, is easy to use, and offers the option of making measurements while heating the sample in a N2 atmosphere. The setup allows X-ray diffraction measurements in Bragg-Brentano mode (i.e., Theta-2Theta measurements where the incident and diffraction arms of the goniometer are coupled). We have a very limited selection of optics for this instrument, so there is little that the user can adjust.

Please contact the equipment responsible if you would like to mount the special sample holder for heating during the measurement.

The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:

XRD Powder in LabManager


Process information

Malvern Panalytical has a large collection of webinars on XRD. You have to register to view them but the amount of email you receive afterwards is modest, so it's worth it in my opinion (Rebecca, July 2022).

  • A tutorial which also mentions sample preparation about half-way through and explains very briefly some of the issues that can arise from displaced samples, not having a thick enough sample layer, odd sized sample particles, etc.

Software

After making a measurement, you will need dedicated software for the data export and analysis.

For data export

On the Cleanroom drive you can find the DataViewer software, which is a very basic program that allows you to view your measurement results and export to other formats, e.g., csv or txt. To install DataViewer, go to the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\XRDMP and click "setup" (XRDMP stands for XRD Measurement Program). This will open a menu that allows you to install both DataViewer and XRDMP Creator. Just choose to install DataViewer. XRDMP Creater is only needed if you have made an agreement with the equipment responsible that you are allowed to create your own measurement routines.

For data analysis

We have a license for the software "HighScore" for Rietveld refinement, allowing quantification of the phase composition. This is so far only available on the support computer by the instrument, but will become available on a remote computer.

Additional software for measurements in a heated atmosphere

If you are going to make measurements in a heated N2 atmosphere, you will need the Nambicon software to control the heater. It is found in the folder O:\CleanroomDrive\_Equipment\XRD Powder\XRD Aeris\Anton Paar Nambicon.


Equipment performance and process related parameters

Equipment XRD Powder
Purpose Crystal structure analysis and thin film thickness measurement
  • Phase ID
  • Crystal Size
  • Crystallinity
X-ray generator

Maximum rated output

600 W

Rated tube voltage

40 kV

Rated tube current

15 mA

Type

Sealed tube

Target

Cu

Focus size

0.4 mm x 12 mm (Line)

Goniometer

Scanning mode

incident / receiver coupled

Goniomenter radius

145 mm

Minimum step size

0.001° (3.6")

Sample stage

Fixed with rotation

Sample size

Powders

Optics Incident side
  • 0.04° soller slit
  • Ni and Cu filter
  • Divergence slits
  • Beam mask
Receiver side
  • 0.04° soller slit
  • Ni filter
Substrates Measurement temperature

May be heated in N2 up to 500 °C

Substrate size

Only for powders

Allowed materials

All materials have to be approved