|-style="background:white; color:black; vertical-align:middle; text-align:center;"
!Microscope
!Location
!Responsible Group
!Objectives
!Ocular
!Special features
!Features
!Camera
!Analysis software
|-
|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Nikon SMZ 1000[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|346-901
|Wet chemistry
|Zoom 0.8x - 8x
|10x
|Stereoscopic microscope
|Episcopic
|No
|No
|-
|-
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!Noco IR[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|346-901
|Wet chemistry
|
*2.5x
*10x
*20x
*50x
|10x
|IR imaging
|
*Polarizer
*Episcopic
*Diascopic
*Brightfield
|IR camera
|No
|-
|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Leica INM100[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|346-901
|Wet chemistry
|
*2.5x
*5x
*10x
*20x
*50x
|10x
|
|
*Episcopic
*Diascopic
*Brightfield
*Darkfield
|DS-Fi2
|NIS-D
|-
|-
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!Nikon Eclipse L200 #2[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|C1
|Thin Film
|
*2.5x
*5x
*10x
*20x
*50x
*100x
|10x
|
|
*Episcopic
*Diascopic
*Brightfield
*Darkfield
|DS-Fi1
|NIS-D
|-
|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Zeiss Jenatech[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|C1
|Thin Film
|
*5x
*10x
*20x
*50x
*100x
|10x
|
|
*Polarizer
*Episcopic
*Diascopic
*Brightfield
|No
|No
|-
|-


|-
|-
|-style="background:white; color:black; vertical-align:middle; text-align:center"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!Nikon Eclipse L200 #1[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|D3
|Thin Film
|
*2.5x
*5x
*10x
*20x
*50x
*100x
|10x
|Motorized stage
|
|
!Nikon SMZ 1000
*Episcopic
!Nikon SMZ 1000
*Diascopic
*Brightfield
*Darkfield
|DS-Fi1
|NIS-BR
|-
|-


|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Leitz Medilux[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|D3
|Thin Film
|
*2.5x
*5x
*10x
*20x
*50x
|10x
|
|
*Episcopic
*Diascopic
*Brightfield
|DX40-274FW
|Kappa Control Center
|-


|-
|-
|-style="background:white; color:black;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!Image
!Nikon Eclipse L200N #3[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|E4
|[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|Lithography
|
*2.5x
*5x
*10x
*20x
*50x
*100x
|10x
|
|
*Polarizer
*Episcopic
*Diascopic
*Brightfield
*Darkfield
|
*DS-Fi2
*C-mount, 0.7x relay
|NIS-D
|-
|-


|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Nikon Eclipse L200N #4[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|E5
|Lithography
|
*2.5x
*5x
*10x
*20x
*50x
*100x
|10x
|
|
*Polarizer
*Episcopic
*Diascopic
*Brightfield
*Darkfield
|
*DS-Fi2
*C-mount, 0.7x relay
|NIS-D
|-


|-
|-
|-style="background:LightGrey; color:black; vertical-align:middle;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!RowHeader1
!Nikon ME 600[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|F1
|Thin Film
|
|
*5x
*10x
*20x
*50x
*100x
|10x
|
|
|
*Polarizer
*Episcopic
*Brightfield
*Darkfield
|DS-Fi2
|NIS-D
|-
|-
|-style="background:LightGrey; color:black; vertical-align:middle; text-align:center;"
!Leica S8 APO[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|F2
|Thin Film
|Zoom 1x - 8x
|10x
|Stereoscopic microscope
|Episcopic
|No
|No
|-
|-


|-
|-
|-style="background:WhiteSmoke; color:black; vertical-align:middle;"
|-style="background:WhiteSmoke; color:black; vertical-align:middle; text-align:center;"
!RowHeader2
!Zeiss Axiotron[[image:Nikon SMZ 1000.jpg|100x100px|thumb|center]]
|F3
|Lithography
|
*5x
*10x
*20x
*50x
|10x
|
|
|
|
*Episcopic
*Diascopic
*Brightfield
*Darkfield
|Infinity X
|DeltaPix
|-
|-