| Line 134: | Line 134: | ||
To get rid of the oscillations we must change from the Fixed pressure mode must to Fixed APC mode. Here, this is no feedback loop: In the transition between phases, the different gas flows, RF powers and APC setting will produce a different pressure that is reached without any overshooting. The price one may have to pay is that the new pressure may be reached at a slower speed. Also, with a pressure setting defined in terms of APC percentage in the recipe, the actual pressures during the process itself will have to be noted manually. | To get rid of the oscillations we must change from the Fixed pressure mode must to Fixed APC mode. Here, this is no feedback loop: In the transition between phases, the different gas flows, RF powers and APC setting will produce a different pressure that is reached without any overshooting. The price one may have to pay is that the new pressure may be reached at a slower speed. Also, with a pressure setting defined in terms of APC percentage in the recipe, the actual pressures during the process itself will have to be noted manually. | ||
= New recipes: | = New recipes= | ||
The group of professor [https://www.dtu.dk/service/telefonbog/person?id=103402&cpid=191195&tab=1 Henri Jansen] at DTU Nanolab has researched the possibilities | |||
[file:DREM2 - Chang_2018_J._Micromech._Microeng._28_105012.pdf] | |||