Specific Process Knowledge/Thin film deposition/Furnace LPCVD TEOS: Difference between revisions
No edit summary |
|||
| Line 6: | Line 6: | ||
==Process Knowledge== | ==Process Knowledge== | ||
Please take a look at the process side for deposition of TEOS oxide: | Please take a look at the process side for deposition of TEOS oxide: | ||
[[Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of | [[Specific Process Knowledge/Thin film deposition/Deposition of Silicon Nitride/Deposition of TEOS using LPCVD|Deposition of TEOS using LPCVD]] | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 08:52, 7 July 2009
This page is in progress!!
LPCVD (Low Pressure Chemical Vapor Deposition) TEOS

At the moment there is one furnace for TEOS oxide depositions at Danchip. The furnace is a Tempress horizontal furnace. The process is a batch process meaning you can run a batch of 10 wafers at a time. The deposition takes place at temperatures of 725 degrees Celsius. The reactive gases are dinitrogenoxide and silane. The LPCVD TEOS has a excellent step coverage and extreamly good for trench filling and the film thickness is very uniform over the wafer. We have two standard LPCVD TEOS processes: One that opens slowly for depositing thick layers (>750nm) and one for deposition of thin layers that opens faster. To get information on how to operate the furnace please read the manual which is uploaded to LabManager. Remember to anneal the TEOS oxide to improve the electrical properties as well as chemical resistance.
Process Knowledge
Please take a look at the process side for deposition of TEOS oxide:
Deposition of TEOS using LPCVD
| Purpose | Deposition of TEOS silicon oxide |
|
|---|---|---|
| Performance | Film thickness| |
|
| Step coverage |
| |
| Film quality |
| |
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Gas flows |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
|