Jump to content

Specific Process Knowledge/Thin film deposition/Physimeca: Difference between revisions

From LabAdviser
Mdyma (talk | contribs)
Mdyma (talk | contribs)
Line 36: Line 36:
|style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"|
|style="background:LightGrey; color:black"|Film thickness||style="background:WhiteSmoke; color:black"|
*10 Å - 5000 Å*
*10 Å - 5000 Å*
*Throw distance 46 cm
 
|-
|-
|style="background:LightGrey; color:black"|Available metals and deposition rates (Å/s)
|style="background:LightGrey; color:black"|Available metals and deposition rates (Å/s)
Line 49: Line 49:
*Silver (Ag)
*Silver (Ag)
|-
|-
!style="background:silver; color:black" align="left" valign="top" rowspan="2"|Process parameter range
!style="background:silver; color:black" align="left" valign="top" rowspan="3"|Process parameter range
|style="background:LightGrey; color:black"|Process Temperature
|style="background:LightGrey; color:black"|Process Temperature
|style="background:WhiteSmoke; color:black"|  
|style="background:WhiteSmoke; color:black"|  
Line 57: Line 57:
|style="background:WhiteSmoke; color:black"|  
|style="background:WhiteSmoke; color:black"|  
* 2x10<sup>-6</sup> mbar
* 2x10<sup>-6</sup> mbar
|-
|style="background:LightGrey; color:black"|Distance between e-beam and substrate
|style="background:WhiteSmoke; color:black"|
* 46 cm
|-
|-
!style="background:silver; color:black" align="left" valign="top" rowspan="3"|Substrates
!style="background:silver; color:black" align="left" valign="top" rowspan="3"|Substrates

Revision as of 10:42, 23 August 2017

Feedback to this page: click here

Physimeca

The Physicmeca, placed in the III-V laboratory, cleanroom A-5.

Physimeca is a system for deposition of metals through electron-beam evaporation, intended for III-V processing.


Wafers are loaded into the system through the load lock and transferred into the deposition chamber. Physimeca allows you to deposit metals on samples of different sizes and shapes. It will also take samples of almost any shape as long as they can fit on the sample holders; there are three different sample holders, one for chips (arbitrary size), one for 2" wafers and one for 4" wafers. The sample holder can be tilted during deposition, but is normally kept in a horizontal orientation.

Six different metals are present at each time in the Physimeca. The metal combination is changed if needed. A list of currently allowed metals is included in the table below; contact the ThinFilm team (thinfilm@danchip.dtu.dk) if you have wishes for other metals.


The user manual and contact information can be found in LabManager:

Physimeca in LabManager




Equipment performance and process related parameters Physimeca

Purpose Deposition of metals
  • E-beam evaporation of metals
Performance Film thickness
  • 10 Å - 5000 Å*
Available metals and deposition rates (Å/s)
  • Gold (Au) 10
  • Chromium (Cr) 5
  • Platinum (Pt) 5
  • Titanium (Ti) 5
  • Nickel (Ni) 5
  • Germanium (Ge) 5
  • Palladium (Pd) 5
  • Silver (Ag)
Process parameter range Process Temperature
  • Less then 80 oC
Process pressure
  • 2x10-6 mbar
Distance between e-beam and substrate
  • 46 cm
Substrates Batch size
  • 2 or 4" wafers
  • Or several smaller pieces
Substrate material allowed
  • III-V materials
  • Si
Materials allowed on the substrate
  • Silicon oxide
  • Silicon (oxy)nitride
  • Photoresist
  • PMMA
  • Mylar

* For thicknesses above 2000 Å special permission is required (contact thinfilm@danchip.dtu.dk).

Calibration of Physimeca - for experienced users only